Fig. 6—(a) A typical entrainment defect in the commercial-purity Mg-alloy casting under the protection of 0.5 pct SF6/air, (b) EDS result of spectrum 1, (c) local magnified outside layer of film, and (d) EDS of spectrum 2.

Fig. 6—(a) A typical entrainment defect in the commercial-purity Mg-alloy casting under the protection of 0.5 pct SF6/air, (b) EDS result of
spectrum 1, (c) local magnified outside layer of film, and (d) EDS of spectrum 2.